DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
| Manufacturer | DuPont Packaging and Industrial Polymers |
| Trade Name | Elvax® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range without the need for plasticizers.Elvax resins can be used alone or to improve the flexibility, resilience and toughness of other resins. Depending on the demands of the particular application, they can be pigmented, foamed, filled, and/or crosslinked. In addition to their performance advantages, Elvax resins are processed easily using conventional thermoplastic processing techniques, i.e., injection molding, extrusion and foaming, as well as rubber processing techniques, i.e., Banbury mixing, foam extrusion and molding.Test specimens except for tensile impact where prepared by compression molding (ASTM D1928, procedure C). Tensile impact samples were injection molded.Processing Information:Molding and ExtrudingModified and unmodified Elvax resins can be processed in conventional thermoplastic and rubber processing equipment. The temperature profile will vary with machine type, size and screw design as well as with part size, thickness or confiation.CompoundingElvax resins are compatible with a variety of other resins and elastomers including polyethylene, polypropylene and styrene-butadiene rubber. Clays and other inorganic fillers can be added to improve abrasion resistance and lower cost.Foaming AgentsElvax resins are readily foamed using chemical or physical blowing agents.Crosslinking AgentsPeroxides such as “Di-Cup”† and “Vul-Cup”† dicumyl peroxide can be used to crosslink or vulcanize Elvax resins.(†Hercules Inc.) Information provided by DuPont.
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
| Vinyl Acetate Content | 28 % | 28 % | TGA |
| Melt Index of Compound | 25 g/10 min | 25 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 80 | 80 | ASTM D2240 |
| Hardness, Shore D | 28 | 28 | ASTM D2240 |
| Tensile Strength, Ultimate | 9.00 MPa | 1310 psi | Type IV, crosshead speed 2 in/min; ASTM D638 |
| 1.40 MPa
@Temperature 49.0 °C
|
203 psi
@Temperature 120 °F
|
Type IV, crosshead speed 2 in/min; ASTM D638 | |
| 23.0 MPa
@Temperature -20.0 °C
|
3340 psi
@Temperature -4.00 °F
|
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638 | |
| Elongation at Break | 850 % | 850 % | Type IV, crosshead speed 2 in/min; ASTM D638 |
| 400 %
@Temperature -20.0 °C
|
400 %
@Temperature -4.00 °F
|
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638 | |
| 500 %
@Temperature 49.0 °C
|
500 %
@Temperature 120 °F
|
Type IV, crosshead speed 2 in/min; ASTM D638 | |
| Modulus of Elasticity | 0.0110 GPa | 1.60 ksi | |
| 0.0460 GPa
@Temperature -20.0 °C
|
6.67 ksi
@Temperature -4.00 °F
|
||
| Flexural Modulus | 0.0110 GPa | 1.60 ksi | ASTM D790 |
| 0.00620 GPa
@Temperature 49.0 °C
|
0.899 ksi
@Temperature 120 °F
|
ASTM D790 | |
| 0.0790 GPa
@Temperature -20.0 °C
|
11.5 ksi
@Temperature -4.00 °F
|
ASTM D790 | |
| Flexural Stiffness | 11.00 MPa | 1595 psi | |
| 46.00 MPa | 6672 psi | ||
| Tensile Impact Strength | 485 kJ/m² | 231 ft-lb/in² | At -20°C; ASTM D1822 |
| 670 kJ/m² | 319 ft-lb/in² | At 23°C; ASTM D1822 | |
| Compression Set | 60 % | 60 % | Method B, 10 days at 25°C; ASTM D395 |
| 100 %
@Temperature 70.0 °C
|
100 %
@Temperature 158 °F
|
Method B, 22 hours; ASTM D395 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 42.0 °C | 108 °F | ASTM D1525 |
| Brittleness Temperature | <= -100 °C | <= -148 °F | ASTM D762 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 121 – 204 °C | 250 – 399 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Cycle time | 0.5-2 minutes | Molding, equipment and part design dependent |
| Vinyl Acetate Content | 28 wt.% |