Eastman Eastar 5445 PCTG Copolyester, Film (discontinued **)
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Category Renewable Recycled Film
Description
Material Notes:
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is transparent. It is tough and resistant to stress whitening. It has fast forming cycles and is easy to form. Eastar PCTG Copolyester 5445 is sterilizable by both gamma radiation and ethylene oxide (ETO) methods. Its scrap can be reused.Applications/UsesBagsCredit cardsGaming cardsIdentification cardsPlastic CardsRigid medicalBlister packagingDebit cardsGift cardsPhone cardsRapid deployment flood wallsSmart cardsKey AttributesExcellent clarityEffective barrier propertiesExcellent colorabilityGood stiffnessSterilizable with ethylene oxide, electron beam, and gamma rays
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D1505 |
Melt Density | 1.08 g/cc
@Temperature 285 °C
|
0.0390 lb/in³
@Temperature 545 °F
|
ASTM D1238 |
Water Vapor Transmission | 7.00 g/m²/day | 0.451 g/100 in²/day | ASTM F372 |
Oxygen Transmission | 11.0 cc-mm/m²-24hr-atm | 27.9 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Carbon Dioxide Transmission | 49.0 cc-mm/m²-24hr-atm | 124 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Thickness | 250 microns | 9.84 mil | ASTM D374 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 45.0 MPa | 6530 psi | ASTM D882 |
Film Tensile Strength at Yield, TD | 44.0 MPa | 6380 psi | ASTM D882 |
Tensile Modulus | 1.60 GPa | 232 ksi | TD; ASTM D882 |
1.60 GPa | 232 ksi | MD; ASTM D882 | |
Coefficient of Friction | 0.50 | 0.50 | ASTM D1894 |
Elmendorf Tear Strength, MD | >= 12.0 g/micron | >= 305 g/mil | ASTM D1922 |
Elmendorf Tear Strength, TD | >= 12.0 g/micron | >= 305 g/mil | ASTM D1922 |
Dart Drop | 1.84 g/micron | 46.7 g/mil | 23°C; ASTM D1709 |
2.16 g/micron | 54.9 g/mil | at -18°C; ASTM D1709 | |
Film Tensile Strength at Break, MD | 57.0 MPa | 8270 psi | ASTM D882 |
Film Tensile Strength at Break, TD | 53.0 MPa | 7690 psi | ASTM D882 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.09 J/g-°C
@Temperature 10.0 °C
|
0.261 BTU/lb-°F
@Temperature 50.0 °F
|
DSC |
1.14 J/g-°C
@Temperature 30.0 °C
|
0.272 BTU/lb-°F
@Temperature 86.0 °F
|
DSC | |
1.64 J/g-°C
@Temperature 100 °C
|
0.392 BTU/lb-°F
@Temperature 212 °F
|
DSC | |
1.86 J/g-°C
@Temperature 180 °C
|
0.445 BTU/lb-°F
@Temperature 356 °F
|
DSC | |
2.16 J/g-°C
@Temperature 290 °C
|
0.516 BTU/lb-°F
@Temperature 554 °F
|
DSC | |
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Glass Transition Temp, Tg | 87.0 °C | 189 °F | ASTM D1525 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.56 | 1.56 | n<sub>D</sub>; ASTM D542 |
Haze | 1.0 % | 1.0 % | ASTM D1003 |
Gloss | 98 % | 98 % | at 60°; ASTM D2457 |
Transmission, Visible | 91 % | 91 % | Total Transmittance; ASTM D1003 |