Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate (discontinued **)
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Category Cellulose Acetate, Molded
Description
Material Notes:
Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of properties – toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. TENITE cellulosic plastics are available in natural, clear, selected ambers, or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. TENITE Cellulose Acetate Butyrate 438-04 contains an odor mask and has a plasticizer level of 4%.Applications: HousewaresTechnical Data Sheet Characteristics: Formula 438 – odor mask. Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.Information provided by Eastman Chemical.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.21 g/cc | 0.0437 lb/in³ | ASTM D792 |
Water Absorption | 1.8 % | 1.8 % | 24 hour immersion; ASTM D570 |
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 97 | 97 | ASTM D785 |
Tensile Strength, Ultimate | 51.0 MPa | 7400 psi | ASTM D638 |
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Elongation at Break | 50 % | 50 % | ASTM D638 |
Flexural Yield Strength | 60.0 MPa | 8700 psi | ASTM D790 |
Flexural Modulus | 1.793 GPa | 260.1 ksi | ASTM D790 |
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
0.800 J/cm
@Temperature -40.0 °C
|
1.50 ft-lb/in
@Temperature -40.0 °F
|
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 – 17.0 µm/m-°C
@Temperature 20.0 °C
|
6.11 – 9.44 µin/in-°F
@Temperature 68.0 °F
|
ASTM D696 |
Specific Heat Capacity | 1.465 J/g-°C | 0.3501 BTU/lb-°F | DSC |
Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | ASTM C177 |
Deflection Temperature at 0.46 MPa (66 psi) | 94.0 °C | 201 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 84.0 °C | 183 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D648 |
Vicat Softening Point | 115 °C | 239 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.475 | 1.475 | ASTM D542 |
Haze | <= 8.5 %
@Thickness 1.52 mm
|
<= 8.5 %
@Thickness 0.0598 in
|
ASTM D1003 |
Transmission, Visible | >= 90 %
@Thickness 1.52 mm
|
>= 90 %
@Thickness 0.0598 in
|
ASTM E308 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+13 – 1.00e+15 ohm-cm | 1.00e+13 – 1.00e+15 ohm-cm | ASTM D257 |
Dielectric Constant | 3.55
@Frequency 1e+6 Hz
|
3.55
@Frequency 1e+6 Hz
|
ASTM D 150 |
Dielectric Strength | 15.25 kV/mm | 387.4 kV/in | ASTM D149 |
Dissipation Factor | 0.080
@Frequency 1e+6 Hz
|
0.080
@Frequency 1e+6 Hz
|
ASTM D150 |