Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.950 g/cc | 0.0343 lb/in³ | Exxon Method |
| Viscosity | 5700 cP
@Temperature 121 °C
|
5700 cP
@Temperature 250 °F
|
melt viscosity; ASTM D-3236 |
| Melt Flow | 5.7 g/10 min | 5.7 g/10 min | Exxon Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 12.0 MPa | 1740 psi | ASTM D638 |
| Elongation at Break | >= 800 % | >= 800 % | ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 72.0 °C | 162 °F | Exxon Method |
| Vicat Softening Point | 150 °C | 302 °F | Softening Point, R&B; ASTM E-28 |