Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent
Manufacturer | Plastcom spol. s r.o. |
Trade Name | SLOVALEN |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Category Polypropylene Glass Bead Filled
Description
Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to themodification. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | |
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | |
Melt Flow | 10 g/10 min
@Load 0.325 kg,
Temperature 270 °C |
10 g/10 min
@Load 0.716 lb,
Temperature 518 °F |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 37.0 MPa | 5370 psi | |
Elongation at Break | 3.0 % | 3.0 % | |
Tensile Modulus | 2.25 GPa | 326 ksi | |
Flexural Strength | 51.0 MPa | 7400 psi | |
Flexural Modulus | 2.18 GPa | 316 ksi | |
Charpy Impact Unnotched | 2.50 J/cm²
@Temperature -20.0 °C
|
11.9 ft-lb/in²
@Temperature -4.00 °F
|
|
4.50 J/cm²
@Temperature 23.0 °C
|
21.4 ft-lb/in²
@Temperature 73.4 °F
|
||
Charpy Impact, Notched | 0.500 J/cm²
@Temperature -20.0 °C
|
2.38 ft-lb/in²
@Temperature -4.00 °F
|
|
0.600 J/cm²
@Temperature 23.0 °C
|
2.86 ft-lb/in²
@Temperature 73.4 °F
|
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 160 °C | 320 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C | 190 °F | |
Vicat Softening Point | 156 °C | 313 °F | B |
Flammability, UL94 | HB | HB | |
Glow Wire Test | 650 °C | 1200 °F |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 – 250 °C | 392 – 482 °F | |
Mold Temperature | 40.0 – 80.0 °C | 104 – 176 °F | |
Drying Temperature | 80.0 °C | 176 °F | |
Dry Time | 2 hour | 2 hour | |
Moisture Content | <= 0.20 % | <= 0.20 % | |
Injection Pressure | 70.0 – 120 MPa | 10200 – 17400 psi |