Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Manufacturer | Solvay Specialty Polymers |
Trade Name | Amodel® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation at temperatures of 230°C. Other features are fast cycling and hot water moldability. This product is particularly suitable to air induction applications within downsized automotive engines such as air induction charge air cooling and exhaust gas recirculation. Features: Fast Molding Cycle; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Laser Weldable; Low Moisture Absorption; LubricatedUses: Automotive Applications; Automotive Under the Hood; Metal ReplacementInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Information provided by Solvay Specialty Polymers.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.57 g/cc | 0.0567 lb/in³ | Dry; ISO 1183 |
Filler Content | 45 % | 45 % | Glass Fiber |
Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | Dry |
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | Dry; ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 327 °C | 621 °F | Dry; ISO 11357-3 |
327 °C | 621 °F | Dry; DSC |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+14 ohm-cm | 5.00e+14 ohm-cm | ASTM D257 |
Dielectric Constant | 3.4
@Frequency 1.00e+6 Hz
|
3.4
@Frequency 1.00e+6 Hz
|
ASTM D150 |
4.3
@Frequency 60.0 Hz
|
4.3
@Frequency 60.0 Hz
|
ASTM D150 | |
Dielectric Strength | 20.0 kV/mm
@Thickness 1.60 mm
|
508 kV/in
@Thickness 0.0630 in
|
ASTM D149 |
Dissipation Factor | 0.019
@Frequency 1.00e+6 Hz
|
0.019
@Frequency 1.00e+6 Hz
|
ASTM D150 |
0.020
@Frequency 60.0 Hz
|
0.020
@Frequency 60.0 Hz
|
ASTM D150 | |
Comparative Tracking Index | 600 V | 600 V | UL 746 |
High Voltage Arc-Tracking Rate, HVTR | 18.0 mm/min | 0.709 in/min | UL 746 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 318 – 324 °C | 604 – 615 °F | |
Front Barrel Temperature | 327 – 332 °C | 621 – 630 °F | |
Melt Temperature | 329 – 343 °C | 624 – 649 °F | |
Mold Temperature | 65.6 – 93.3 °C | 150 – 200 °F | |
Drying Temperature | 120 °C
@Time 14400 sec
|
248 °F
@Time 4.00 hour
|
|
Moisture Content | <= 0.045 % | <= 0.045 % |
Descriptive Properties | Value | Comments |
---|---|---|
Additive | Heat Stabilizer | |
Lubricant | ||
Mold Release | ||
Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
Latin America | ||
North America | ||
Color | Black | |
Form | Pellets | |
Processing Technique | Water-Heated Mold Injection Molding |