Material Notes:
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It’s a soft, elastomeric polyolefin based, completely recyclable, colorable & non-hygroscopic thermoplastics elastomer material.Information provided by Stellarchem Polymer & Industrial
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Particle Mesh Size | 80 – 150 Mesh | 80 – 150 Mesh | |
Melt Flow | 90 g/10 min | 90 g/10 min | JIS K7210 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 10 | 10 | JIS K6301 |
Tensile Strength, Ultimate | 1.18 MPa | 171 psi | JIS K6301 |
Elongation at Break | 983 % | 983 % | JIS K6301 |
100% Modulus | 0.000980 GPa | 0.142 ksi | JIS K6301 |
300% Modulus | 0.0000981 GPa | 0.0142 ksi | JIS K6301 |
Tear Strength | 4.02 kN/m | 23.0 pli | JIS K6301-B |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 200 – 220 °C | 392 – 428 °F | Metering Temperature, Extrusion |
Rear Barrel Temperature | 160 – 180 °C | 320 – 356 °F | Injection Molding |
160 – 180 °C | 320 – 356 °F | Extrusion | |
Middle Barrel Temperature | 180 – 200 °C | 356 – 392 °F | Injection Molding |
180 – 200 °C | 356 – 392 °F | Transition, Extrusion | |
Front Barrel Temperature | 200 – 220 °C | 392 – 428 °F | Injection Molding |
220 – 230 °C | 428 – 446 °F | Extrusion | |
Nozzle Temperature | 220 – 230 °C | 428 – 446 °F | Injection Molding |
Die Temperature | 195 – 210 °C | 383 – 410 °F | Extrusion |
Melt Temperature | 150 – 230 °C | 302 – 446 °F | Injection Molding |
150 – 230 °C | 302 – 446 °F | Extrusion | |
Mold Temperature | 25.0 – 40.0 °C | 77.0 – 104 °F | Injection Molding |
Injection Pressure | 5.00 – 40.0 MPa | 725 – 5800 psi | Injection Molding |
Back Pressure | 0.500 – 1.00 MPa | 72.5 – 145 psi | Injection Molding |
Screw Speed | 60 – 100 rpm | 60 – 100 rpm | Extrusion |
100 – 200 rpm | 100 – 200 rpm | Injection Molding |