ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin
| Manufacturer | Exxon Chemical |
| Trade Name | Escorene® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: Yes Applications:FoamsInjection MoldingProfile ExtrusionShoe SolesInformation provided by ExxonMobil Chemical
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.935 g/cc | 0.0338 lb/in³ | ExxonMobil Method |
| Vinyl Acetate Content | 18.2 % | 18.2 % | ExxonMobil Method |
| Melt Flow | 2.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C |
2.00 g/10 min
@Load 4.76 lb,
Temperature 374 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 76 | 76 | 15s; ASTM D2240 |
| Hardness, Shore D | 36 | 36 | 15s; ASTM D2240 |
| Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D638 |
| Tensile Strength, Yield | 5.24 MPa | 760 psi | ASTM D638 |
| Elongation at Break | >= 800 % | >= 800 % | ASTM D638 |
| Elongation at Yield | 260 % | 260 % | ASTM D638 |
| Flexural Modulus | 0.0607 GPa | 8.80 ksi | 1% secant; ASTM D790 |
| Impact Test | 17.6 J
@Temperature 23.0 °C
|
13.0 ft-lb
@Temperature 73.4 °F
|
Instrument Impact, Total Energy; ASTM D3763 |
| 35.3 J
@Temperature -40.0 °C
|
26.0 ft-lb
@Temperature -40.0 °F
|
Instrumented Impact, Total Energy; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 87.2 °C | 189 °F | Peak Melting Temperature; ExxonMobil Method |
| Vicat Softening Point | 63.9 °C | 147 °F | ASTM D1525 |