ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer (discontinued **)
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristics. This grade of Vyram TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Information provided by Advanced Elastomer Systems
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.980 g/cc | 0.980 g/cc | 23°C; ASTM D792 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 85 | 85 | .12 in; ASTM D2240 |
88 | 88 | 302°F, 168 hr; ASTM D573 | |
Tensile Strength at Break | 9.93 MPa | 1440 psi | Across Flow; ASTM D412 |
11.42 MPa | 1656 psi | 302°F, 168 hr; ASTM D573 | |
Tensile Strength, Ultimate | 5.31 MPa | 770 psi | Across Flow; ASTM D412 |
Elongation at Break | 650 % | 650 % | Across Flow; ASTM D412 |
669.5 % | 669.5 % | 302°F, 168 hr; ASTM D573 | |
Tear Strength | 42.1 kN/m | 240 pli | 73°F, Die C; ASTM D624 |
Compression Set | 54 % | 54 % | 73°F, 22 hr; ASTM D395 |
59 % | 59 % | 212°F, 70 hr; ASTM D395 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM 746 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 175 – 230 °C | 347 – 446 °F | |
Rear Barrel Temperature | 188 °C | 370 °F | |
Middle Barrel Temperature | 191 °C | 375 °F | |
Front Barrel Temperature | 193 °C | 380 °F | |
Nozzle Temperature | 199 °C | 390 °F | |
Die Temperature | 216 °C | 420 °F | Extrusion |
Melt Temperature | 177 – 204 °C | 350 – 400 °F | Extrusion |
204 °C | 400 °F | ||
Mold Temperature | 10.0 – 51.7 °C | 50.0 – 125 °F | Processing |
Drying Temperature | 82.2 °C | 180 °F | |
Dry Time | 3 hour | 3 hour | |
Moisture Content | 0.080 % | 0.080 % | |
Back Pressure | 0.345 – 0.689 MPa | 50.0 – 100 psi | Processing |
5.00 – 20.0 MPa | 725 – 2900 psi | Extrusion | |
Clamp Pressure | 41.4 – 68.9 MPa | 6000 – 10000 psi | |
Vent Depth | 0.00254 cm | 0.00100 in | |
Cushion | 0.317 – 0.635 cm | 0.125 – 0.250 in | |
Screw Speed | 100 – 200 rpm | 100 – 200 rpm |
Descriptive Properties | Value | Comments |
---|---|---|
Change in Mass in IRM 903 Oil at 257°F for 70 hr | 49 | |
Color | Black | |
Form | Pellets | |
Injection Rate | Fast | |
Maximum Regrind % | 20 | |
Screw Compression Ratio | 2:1 – 2.5:1 | |
Screw L/D Ratio | 16:1 – 20:1 |