DuPont™ Surlyn® 1707 Sodium Ionomer
Manufacturer | DuPont |
Trade Name | Surlyn® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Category Ionomer, Film Grade
Description
Material Notes:
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1707 complies with Food and Drug Administration Regulation 21 CFR 177.1330(a) – – Ionomeric resins, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c) of the Regulation.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792, ISO 1183 |
Melt Flow | 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C |
0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F |
ASTM D1238, ISO 1133 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 51.0 °C | 124 °F | Freezing Point; ASTM D3417, ISO 3146 |
92.0 °C | 198 °F | ASTM D3417, ISO 3146 | |
Vicat Softening Point | 58.0 °C | 136 °F | ASTM D1525, ISO 306 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | <= 285 °C | <= 545 °F | |
Feed Temperature | 135 °C | 275 °F | Blown Film Coextrusion |
160 °C | 320 °F | Cast Film/Sheet Processing | |
Zone 2 | 160 °C | 320 °F | Blown Film Coextrusion |
210 °C | 410 °F | Cast Film/Sheet Processing | |
Zone 3 | 185 °C | 365 °F | Blown Film Coextrusion |
235 °C | 455 °F | Cast Film/Sheet Processing | |
Zone 4 | 185 °C | 365 °F | Blown Film Coextrusion |
235 °C | 455 °F | Cast Film/Sheet Processing | |
Zone 5 | 185 °C | 365 °F | Blown Film Coextrusion |
235 °C | 455 °F | Cast Film/Sheet Processing | |
Adapter Temperature | 185 °C | 365 °F | Blown Film Coextrusion |
235 °C | 455 °F | Cast Film/Sheet Processing | |
Die Temperature | 185 °C | 365 °F | Blown Film Coextrusion |
235 °C | 455 °F | Cast Film/Sheet Processing | |
Melt Temperature | 160 – 260 °C | 320 – 500 °F | Blown/Cast Film Processing |