DuPont Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
| Manufacturer | DuPont Packaging and Industrial Polymers |
| Trade Name | Elvax® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences in compatibility. To minimize viscosity changes in hot melt blends during processing, Elvax® 40W also contains butylated hydroxytoluene(BHT). Elvax®40W is supplied in pellet form and to prevent the pellets from blocking, low levels of an amide wax have been added to the polymer.Typical Applications: Laminating adhesives for a variety of substrates including plastics and films. This grade provides the extended open time often needed in industrial assemblyLacquers for wood, metal, metal foils, paper, and filmsFabric and decal coatingsHeat-seal coatings for backing card stock used in blister packagingWood primers and sealers. Combinations of Elvax® 40W and nitrocellulose form the basis for wood sealers offering toughness and good intercoat adhesion Elvax® 40W is also suggested for use as a modifier in: Elastomer-based hot melt and hot melt pressure-sensitive adhesion formulationsNatural and synthetic elastomers to improve resistance to ozone crackingCaulks and sealants, including those based on asphaltAsphalt road repairing compositions for resurfacing, patching, and crack sealing to improve low temperature flexibility, strength properties, and adhesionTraffic paint formulationsSolvent-based and wax-based inksInformation provided by DuPont.
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D1505 |
| Viscosity Measurement | 0.70
@Temperature 30.0 °C
|
0.70
@Temperature 86.0 °F
|
Inherent, 0.25 g/100mL toluene |
| Vinyl Acetate Content | 40 % | 40 % | DuPont Method |
| Melt Index of Compound | 52 g/10 min | 52 g/10 min | ASTM D1238, modified |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 40 | 40 | 10 seconds, Shore A-2; ASTM D2240 |
| Tensile Strength at Break | 4.80 – 6.20 MPa | 696 – 899 psi | Samples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D1708 |
| Elongation at Break | 1000 – 1300 % | 1000 – 1300 % | Samples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D1708 |
| Tensile Modulus | 0.00300 GPa | 0.435 ksi | Samples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Ring & Ball Softening Point | 104 °C | 219 °F | ASTM E28 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Antioxidant | 550 ppm | BHT |
| Odor | Slight | |
| Residual VA Monomer, wt% | <0.3 | |
| Vinyl Acetate Content | 40 wt.% | DuPont Method |