Advanced Elastomer Systems Santoprene® 453-45 Thermoplastic Rubber (discontinued **)
Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber |
Manufacturer | |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
A colorable thermoplastic flame retardant wire and cable elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques.Key Features: Meets UL 1277 requirements of both insulation and jacket for control and tray; UL 62 Bulletin listed; Wire and cable rating: 105°C (221°F) dry, 75°C (167°F) wet and 60°C (140°F) oil; Limiting oxygen index, 24.5% (passes VW-1, IEEE 383); EM 60 at 75°C (167°F): 1 day SIC = 2.47; % change in SIC, 1 to 14 days = 1.07; % change in SIC, 7 to 14 days = .50; Stability factor, 14 days = 0.07; IR constant @ 15.6°C (60°F) = >100,000Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.22 g/cc | 0.0441 lb/in³ | TPE-0105 (ASTM D792) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 45 | 45 | 5 Second; TPE-0169 (ASTM D 2240) |
Tensile Strength, Ultimate | 14.5 MPa | 2100 psi | TPE-0153 (ASTM D 412) |
Elongation at Break | 540 % | 540 % | TPE-0153 (ASTM D 412) |
100% Modulus | 0.00780 GPa | 1.13 ksi | TPE-0153 (ASTM D 412) |
Tear Strength | 62.7 kN/m | 358 pli | 62.7 kN/m at 23°C. Value at 100°C is 36.9 kN/m. TPE-0056 (ASTM D 624) |
Compression Set | 34 % | 34 % | 23°C, 168 hrs.; TPE-0016 (ASTM D 412) |
71 %
@Temperature 100 °C
|
71 %
@Temperature 212 °F
|
168 hrs.; TPE-0016 (ASTM D 412) | |
Tensile Set | 42 % | 42 % | 23°C, 168 hrs.; TPE-0053 (ASTM D 412) |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 105 °C | 221 °F | Wire and Cable Rating Dry |
Brittleness Temperature | <= -42.0 °C | <= -43.6 °F | TPE-0089 (ASTM D 746) |
Oxygen Index | 24.5 % | 24.5 % |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 – 232 °C | 351 – 450 °F | |
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Dry Time | 3 hour | 3 hour |