ExxonMobil Label-Lyte® 30 LLG-101 Clear OPP Film
Manufacturer | Exxon Chemical |
Trade Name | Label-Lyte® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Categories Polypropylene (PP), Polypropylene, Film Grade, Thermoplastic
Description
Material Notes:
Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied as outer webs to other films. It is formulated with a proprietary non-migratory slip system. The treated clear layer is the intended print and laminating surface. The machinable high gloss layer is receptive to hot melt adhesive.Availability: Latin America, North America and South AmericaKey Features: Outstanding clarity and glossExcellent ink adhesion with most solvent-based and water-based ink systemsExcellent bond strength with most laminating adhesivesContains non-migratory slip system for outstanding performance on roll-fed labeling machinesGood hot melt adhesionApplications:Beverage, CarbonatedBeverage, Mineral WatersDairy ProductsDry Foods and Beverage Powders Health and Beauty CareHousehold and DetergentsIndustrial Uses: Reel-Fed Labels Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic PrintingInformation provided by ExxonMobil Chemical
Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
Coating Weight | 27.4 g/m² | 17.1 lb/ream | ExxonMobil Method |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Elongation at Break, MD | 183 % | 183 % | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
Film Elongation at Break, TD | 46 % | 46 % | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
Coefficient of Friction | 0.18 | 0.18 | Machinable; ExxonMobil Method |
Film Tensile Strength at Break, MD | 124.11 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
Film Tensile Strength at Break, TD | 241.32 MPa | 35000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Shrinkage, MD | 4.0 % | 4.0 % | at 275°F; ExxonMobil Method |
Shrinkage, TD | 4.0 % | 4.0 % | at 275°F; ExxonMobil Method |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Haze | 2.0 % | 2.0 % | ExxonMobil Method |
Gloss | 87 % | 87 % | 45°, Machinable Surface; ExxonMobil Method |
Transmission, Visible | 90 % | 90 % | clear; thickness not quantified |
Descriptive Properties | Value | Comments |
---|---|---|
Wetting Tension | 0.83 receding COS theta | Print Surface |
Yield | 25500 in2/lb |