ExxonMobil Metallyte™ 18MM882 OPP Film
| Manufacturer | Exxon Chemical |
| Trade Name | Metallyte™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
Categories Polypropylene (PP), Polypropylene, Film Grade, Thermoplastic
Description
Material Notes:
Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, flavors and aromas. The non-metalized PE compatible layer is designed for excellent adhesion of polyethylene for extrusion coating or extrusion laminations. This layer will lap seal to a range of polyethylene films. This film has excellent and consistent flip characteristics and an be treated for printing and adhesive laminating.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South AmericaKey Features:Outstanding oxygen barrier Outstanding moisture and light barriersOutstanding aroma and flavor barrierEasily converted on the meal sideExcellent puncture resistanceLap sealable to PEStable CoF on unmetallized surfaceFeatures:Flavor & Aroma BarrierGas BarrierGrease ResistantLap Sealable to PELight BarrierMoisture BarrierOxygen BarrierPuncture ResistantTwo Side ProcessableApplications:Biscuits/Cookie/CrackersConfectionery, Chocolate Crisps and SnacksDry Foods and Beverage PowdersHealth and Beauty CareHousehold and DetergentsPet Food Uses: HFFS Flexible PackagingLidding – Flexible PackagingPouches – Flexible PackagingPre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Extrusion Coating, Middle Web Extrusion Lamination and Outer Web Adhesive LaminationInformation provided by ExxonMobil
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Water Vapor Transmission | 0.0931 g/m²/day
@Temperature 38.0 °C
|
0.00600 g/100 in²/day
@Temperature 100 °F
|
90% RH; ExxonMobil Method |
| Oxygen Transmission Rate | 0.101 cc/m²/day
@Temperature 23.0 °C
|
0.00650 cc/100 in²/day
@Temperature 73.4 °F
|
ExxonMobil Method |
| Thickness | 18.0 microns | 0.710 mil | ExxonMobil Method |
| Coating Weight | 16.2 g/m² | 10.1 lb/ream | ExxonMobil Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
| Film Tensile Strength at Break, TD | 234 MPa | 34000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Shrinkage, MD | 4.5 %
@Temperature 135 °C,
Time 432 sec |
4.5 %
@Temperature 275 °F,
Time 0.120 hour |
ExxonMobil Method |
| Shrinkage, TD | 4.5 %
@Temperature 135 °C,
Time 432 sec |
4.5 %
@Temperature 275 °F,
Time 0.120 hour |
ExxonMobil Method |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Optical Density | 2.8 | 2.8 | ExxonMobil Method |
| Transmission, Visible | 0.20 % | 0.20 % | ExxonMobil Method |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Yield | 42900 in2/lb |