Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer (discontinued **)

Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union

Description

Material Notes:
Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature application, where higher strength & stiffness needed in load bearing application. Excellent wear resistance. Typical applications include electronic chip carrier trays, conductive flooring, and parts for electronic business machines.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc

1.42 g/cc

Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
Linear Mold Shrinkage, Flow 0.0090 cm/cm

0.0090 in/in

410°C nozzle, 220°C mold
Linear Mold Shrinkage, Transverse 0.012 cm/cm

0.012 in/in

410°C nozzle, 220°C mold

 

Mechanical Properties Metric English Comments
Hardness, Rockwell M 104

104

ASTM D785
Hardness, Shore D 87

87

Tensile Strength, Yield 160 MPa

23200 psi

ASTM D638
Elongation at Break 2.3 %

2.3 %

ASTM D638
Tensile Modulus 16.0 GPa

2320 ksi

ASTM D638
Flexural Strength 250 MPa

36300 psi

ASTM D790
Flexural Modulus 12.9 GPa

1870 ksi

ASTM D790
Izod Impact, Notched 0.350 – 0.400 J/cm

0.656 – 0.749 ft-lb/in

ASTM D256
Izod Impact, Unnotched 3.50 J/cm

6.56 ft-lb/in

ASTM D256

 

Thermal Properties Metric English Comments
Melting Point 370 – 372 °C

698 – 702 °F

DSC
Deflection Temperature at 1.8 MPa (264 psi) 340 °C

644 °F

Glass Transition Temp, Tg 152 – 154 °C

306 – 309 °F

DSC/onset
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in

 

Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm

1.00e+8 ohm-cm

ASTM D257
Surface Resistivity per Square 1.00e+6 ohm

1.00e+6 ohm

ASTM D257

 

Processing Properties Metric English Comments
Processing Temperature 390 – 425 °C

734 – 797 °F

Nozzle Temperature 425 °C

797 °F

Mold Temperature 200 – 220 °C

392 – 428 °F

Drying Temperature 150 °C

302 °F

Dry Time 4 – 6 hour

4 – 6 hour

 

Descriptive Properties Value Comments
Hopper/ Throat Temperature 60-80°C

Nominal Granule Diameter 2.0 – 3.5 mm

Granules of uniform cut and color
Nominal Granule Length 2.0 – 4.0 mm

No longs greater than 8.0 mm