Perstorp Compounds 371 Urea-Formaldehyde w/ cellulose filler
Manufacturer | Perstorp Compounds |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Category Uncategorized
Description
Material Notes:
Information provided by Perstorp Compounds Inc.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0070 – 0.0090 cm/cm | 0.0070 – 0.0090 in/in | DIN 53 464 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 55.0 MPa | >= 7980 psi | ISO 178 |
Flexural Strength | >= 105 MPa | >= 15200 psi | ISO 178 |
Charpy Impact Unnotched | >= 0.800 J/cm² | >= 3.81 ft-lb/in² | ISO 179 |
Charpy Impact, Notched | >= 0.160 J/cm² | >= 0.761 ft-lb/in² | ISO 179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | >= 130 °C | >= 266 °F | ISO 175 |
Deflection Temperature at 8.0 MPa | >= 90.0 °C | >= 194 °F | ISO 175 |
Flammability, UL94 | V-1 | V-1 | |
Oxygen Index | >= 30 % | >= 30 % | ASTM D2863 |
Shrinkage | 0.90 – 1.4 % | 0.90 – 1.4 % | Post Shrinkage; DIN 53 464 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | DIN 53 483 |
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | DIN 53 482 |
Dielectric Constant | 5.0 | 5.0 | DIN 53 483 |
Dissipation Factor | <= 0.10
@Frequency 1000 Hz
|
<= 0.10
@Frequency 1000 Hz
|
tan delta; DIN 53 483 |
Comparative Tracking Index | >= 600 V | >= 600 V | IEC 112 |
Descriptive Properties | Value | Comments |
---|---|---|
Glow Bar 960°C 180 sec | passes | IEC 707 |
Water Absorption [mg] | <250 | DIN 53 495/23°C 96h |