Material Notes:
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 – 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with the halogen flame retardant. Application – stadium seats with guaranteed life-cycle of the mechanical and surface properties, electrical industry – terminals, coil forms, covers of electrotools, guides. Fulfills 960°C glow wire and flammability in accordance with UL 94 V2. Concerning flammability, it complies with the building norm DIN 4102-B2. Delivered in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.930 g/cc | 0.0336 lb/in³ | STN 64 0111 |
Linear Mold Shrinkage | 0.0244 cm/cm | 0.0244 in/in | STN 64 0808 |
Linear Mold Shrinkage, Transverse | 0.0239 cm/cm | 0.0239 in/in | STN 64 0808 |
Melt Flow | 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C |
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F |
STN EN ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 28.0 MPa | 4060 psi | STN EN ISO 527-2 |
Elongation at Break | 20 % | 20 % | STN EN ISO 527-2 |
Tensile Modulus | 1.20 GPa | 174 ksi | STN EN ISO 527-2 |
Flexural Strength | 35.0 MPa | 5080 psi | STN EN ISO 178 |
Flexural Modulus | 1.00 GPa | 145 ksi | STN EN ISO 178 |
Charpy Impact Unnotched | 11.0 J/cm²
@Temperature -20.0 °C
|
52.3 ft-lb/in²
@Temperature -4.00 °F
|
STN EN ISO 179 |
NB
@Temperature 23.0 °C
|
NB
@Temperature 73.4 °F
|
STN EN ISO 179 | |
Charpy Impact, Notched | 0.400 J/cm²
@Temperature -20.0 °C
|
1.90 ft-lb/in²
@Temperature -4.00 °F
|
STN EN ISO 179 |
0.900 J/cm²
@Temperature 23.0 °C
|
4.28 ft-lb/in²
@Temperature 73.4 °F
|
STN EN ISO 179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | STN EN ISO 75/A |
Vicat Softening Point | 110 °C | 230 °F | B; STN EN ISO 306 |
Flammability, UL94 | V-2 | V-2 | |
Glow Wire Test | 960 °C | 1760 °F | STN IEC 60695-2-10 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | STN IEC 60093 |
Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | STN IEC 60093 |
Dielectric Strength | 24.0 kV/mm | 610 kV/in | STN IEC 60243 |
Comparative Tracking Index | 450 V | 450 V | STN 34 6468 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 – 250 °C | 392 – 482 °F | |
Mold Temperature | 30.0 – 50.0 °C | 86.0 – 122 °F | |
Injection Pressure | 50.0 – 80.0 MPa | 7250 – 11600 psi |