Material Notes:
FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application – electrical industry – terminals, coil forms, covers of electrotools, guides. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.04 g/cc

0.0376 lb/in³

Linear Mold Shrinkage 0.0184 cm/cm

0.0184 in/in

Linear Mold Shrinkage, Transverse 0.0168 cm/cm

0.0168 in/in

Melt Flow 10 g/10 min

@Load 0.325 kg,
Temperature 270 °C
10 g/10 min

@Load 0.716 lb,
Temperature 518 °F

 

Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa

3630 psi

Elongation at Break 5.0 %

5.0 %

Tensile Modulus 3.20 GPa

464 ksi

Flexural Strength 44.0 MPa

6380 psi

Flexural Modulus 3.00 GPa

435 ksi

Charpy Impact Unnotched 1.00 J/cm²

@Temperature -20.0 °C
4.76 ft-lb/in²

@Temperature -4.00 °F
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.150 J/cm²

@Temperature -20.0 °C
0.714 ft-lb/in²

@Temperature -4.00 °F
0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F

 

Thermal Properties Metric English Comments
Melting Point 160 °C

320 °F

Deflection Temperature at 1.8 MPa (264 psi) 133 °C

271 °F

Vicat Softening Point 157 °C

315 °F

B
Flammability, UL94 V-0

V-0

Glow Wire Test 960 °C

1760 °F

 

Processing Properties Metric English Comments
Melt Temperature 200 – 250 °C

392 – 482 °F

Mold Temperature 40.0 – 70.0 °C

104 – 158 °F

Injection Pressure 70.0 – 120 MPa

10200 – 17400 psi