Teknor Apex Sarlink® 4190 Thermoplastic Elastomer
Manufacturer | Teknor Apex Company |
Trade Name | Sarlink® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical resistance and high temperature performance. It can be easily processed by injection molding, blow molding or extrusion for various applications such as boots and bellows, seals, gaskets as well as other profiles and articles.Processing and Handling (See more in property table)Sarlink® 4190 is a polypropylene based elastomer, which can be processed on conventional thermoplastic equipment for injection molding, extrusion and blow molding. This product has a wide processing window in most applications. Melt temperatures from 360°F to 430°F can be used. Do not exceed 450°F. Drying is recommended for extrusion and blow molding and any time the material is used from an unsealed package. Extrusion screen pack is 20 to 60 mesh.PURGINGThis product has excellent melt stability. Empty the barrel for idle periods of thirty (30) minutes or longer. Purge thoroughly before and after use of this product with polyethylene or polypropylene.RECYCLING/REGRINDThis product can be reprocessed. Physical properties are generally not degraded. Dry regrind prior to reprocessing. COLORINGThe use of polyolefin based color concentrates is recommended. Apply back pressure in injection molding to disperse color.BONDING/ASSEMBLYThermal bonding techniques can be used to form high strength bonds. Adhesive bonding can be achieved with specialized adhesives. Bond strength is limited due to the polypropylene base of this material.STORAGE and HANDLINGThis product is available in 55 lb. foil lined bags (up to 2,200 lbs. per pallet) or 1,100 lb. polyethylene lined gaylords. It has a storage life at normal temperatures of several years. Please refer to the Material Safety Data Sheet for this grade prior to first time handling.Sarlink® was sold from DSM to Teknor Apex
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Viscosity | 360000 cP
@Shear Rate 206 1/s,
Temperature 200 °C |
360000 cP
@Shear Rate 206 1/s,
Temperature 392 °F |
ASTM D3835 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 86 | 86 | extruded sample; 5 sec. delay; ASTM D2240 |
90 | 90 | injection molded sample; 5 sec. delay; ASTM D2240 | |
Tensile Strength at Break | 13.00 MPa | 1885 psi | Die C; Flow direction; ASTM D412 |
14.80 MPa | 2147 psi | Die C; Cross direction; ASTM D412 | |
Elongation at Break | 524 % | 524 % | Die C; Flow direction; ASTM D412 |
577 % | 577 % | Die C; Cross direction; ASTM D412 | |
100% Modulus | 0.00670 GPa | 0.972 ksi | Die C; Cross direction; ASTM D412 |
0.00770 GPa | 1.12 ksi | Die C; Flow direction; ASTM D412 | |
Tear Strength | 71.0 kN/m | 405 pli | Die C; Cross direction; ASTM D624 |
Compression Set | 39 % | 39 % | 22h/23°C; ASTM D395B |
59 %
@Temperature 100 °C
|
59 %
@Temperature 212 °F
|
22hr; ASTM D395B |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 182 – 204 °C | 360 – 400 °F | Extrusion |
177 – 216 °C | 350 – 420 °F | Injection Molding | |
Middle Barrel Temperature | 182 – 204 °C | 360 – 400 °F | Extrusion Transition Zone |
177 – 216 °C | 350 – 420 °F | Injection Molding | |
188 – 210 °C | 370 – 410 °F | Extrusion Metering Zone | |
Front Barrel Temperature | 177 – 216 °C | 350 – 420 °F | Injection Molding |
188 – 210 °C | 370 – 410 °F | Extrusion | |
Nozzle Temperature | 188 – 221 °C | 370 – 430 °F | Injection Molding |
Die Temperature | 193 – 216 °C | 380 – 420 °F | Extrusion |
Melt Temperature | 182 – 221 °C | 360 – 430 °F | Injection Molding |
193 – 216 °C | 380 – 420 °F | Extrusion | |
Mold Temperature | 10.0 – 65.6 °C | 50.0 – 150 °F | Injection Molding |
Roll Temperature | 21.1 – 48.9 °C | 70.0 – 120 °F | Extrusion |
Drying Temperature | 82.2 °C | 180 °F | |
Dry Time | 3 hour | 3 hour | |
Injection Pressure | 0.0689 – 1.03 MPa | 10.0 – 150 psi | Injection Molding Back Pressure |
Screw Speed | 100 – 200 rpm | 100 – 200 rpm | Injection Molding |