Ensinger TECASINT 5011 Polyimide (PI)
| Manufacturer | Ensinger |
| Trade Name | TECASINT |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
Description
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main FeaturesHigh thermal and mechanical capacityHigh gamma radiation resistanceGood chemical resistanceEasily machinedGood electrical insulationVery creep resistantWear resistanceLow coefficient of thermal expansionFlame retardant according to UL94 V-0Sensitive to hydrolysis in higher thermal rangeApplicationsCryogenicsAircraft and aerospace industriesElectrical engineeringNuclear and vacuum technologyMechanical engineeringChemical plant engineeringPreferred FieldsSwitch parts, seals, connector, housing, lead backerInformation Provided by Ensinger, Inc.
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.38 g/cc
@Temperature 23.0 °C
|
0.0499 lb/in³
@Temperature 73.4 °F
|
DIN 53 479 |
| Water Absorption | 4.17 %
@Temperature 80.0 °C
|
4.17 %
@Temperature 176 °F
|
3 week saturation; EN ISO 62 |
| 0.69 %
@Temperature 23.0 °C,
Time 86400 sec |
0.69 %
@Temperature 73.4 °F,
Time 24.0 hour |
EN ISO 62 | |
| 2.24 %
@Temperature 80.0 °C,
Time 86400 sec |
2.24 %
@Temperature 176 °F,
Time 24.0 hour |
EN ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 91
@Temperature 23.0 °C
|
91
@Temperature 73.4 °F
|
DIN 53 505 |
| Tensile Strength, Yield | 110 MPa
@Temperature 23.0 °C
|
16000 psi
@Temperature 73.4 °F
|
EN ISO 527 |
| Elongation at Break | 5.5 %
@Temperature 23.0 °C
|
5.5 %
@Temperature 73.4 °F
|
EN ISO 527 |
| Elongation at Yield | 4.3 % | 4.3 % | Flexural; EN ISO 178 |
| Tensile Modulus | 4.50 GPa
@Temperature 23.0 °C
|
653 ksi
@Temperature 73.4 °F
|
EN ISO 527 |
| Flexural Strength | 162 MPa
@Temperature 23.0 °C
|
23500 psi
@Temperature 73.4 °F
|
EN ISO 178 |
| Flexural Modulus | 4.24 GPa
@Temperature 23.0 °C
|
615 ksi
@Temperature 73.4 °F
|
EN ISO 178 |
| Compressive Strength | 474 MPa
@Temperature 23.0 °C
|
68700 psi
@Temperature 73.4 °F
|
EN ISO 604 |
| Charpy Impact Unnotched | 3.74 J/cm² | 17.8 ft-lb/in² | EN ISO 179 |
| Compression Set | 98 % | 98 % | Compression at Break; EN ISO 604 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 48.0 µm/m-°C
@Temperature 50.0 – 200 °C
|
26.7 µin/in-°F
@Temperature 122 – 392 °F
|
DIN 53 752 |
| Glass Transition Temp, Tg | 340 °C | 644 °F | DMTA |
| Flammability, UL94 | V-0 | V-0 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Sandy | |
| DIN-Abbreviation | PAI CF |