ExxonMobil Geolast® 701-70 Thermoplastic Elastomer

Manufacturer Exxon Chemical
Trade Name Geolast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union

Description

Material Notes:
A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applications. This grade of Geolast TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Recyclable. Designed for improved fluid resistance.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

1.00 g/cc

23°C; ASTM D792

 

Mechanical Properties Metric English Comments
Hardness, Shore A 70

70

.12 in; ASTM D2240
71

71

Air at 257°F, 168 hr; ASTM D573
Tensile Strength at Break 4.45 MPa

645 psi

257°F, 70 hr in IRM 903 Oil; ASTM D471
5.93 MPa

860 psi

Across Flow; ASTM D412
6.700 MPa

971.8 psi

Air at 257°F, 168 hr; ASTM D573
Tensile Strength, Ultimate 3.31 MPa

480 psi

Across Flow; ASTM D412
Elongation at Break 189.8 %

189.8 %

257°F, 70 hr in IRM 903 Oil; ASTM D471
249.6 %

249.6 %

Air at 257°F, 168 hr; ASTM D573
260 %

260 %

Across Flow; ASTM D412
Tear Strength 18.9 kN/m

108 pli

73°C, Die C; ASTM D624
Compression Set 25 %

25 %

158°F, 22 hr; ASTM D395
33 %

33 %

257°F, 70 hr; ASTM D395

 

Thermal Properties Metric English Comments
Brittleness Temperature -37.2 °C

-35.0 °F

ASTM D746

 

Processing Properties Metric English Comments
Processing Temperature 175 – 230 °C

347 – 446 °F

Melt Temperature <= 102 °C

<= 215 °F

 

Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 0.72

Color Black

Form Pellets