Plastcom SLOVALEN PH 49 GF 40 PP, 40% glass fibre

Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union

Description

Material Notes:
PP homopolymer for injection moulding, chemically strengthened with 40% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry.Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.20 g/cc

0.0434 lb/in³

Linear Mold Shrinkage 0.0189 cm/cm

0.0189 in/in

Linear Mold Shrinkage, Transverse 0.0165 cm/cm

0.0165 in/in

Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F

 

Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa

14500 psi

Elongation at Break 3.0 %

3.0 %

Tensile Modulus 8.00 GPa

1160 ksi

Flexural Strength 130 MPa

18900 psi

Flexural Modulus 6.50 GPa

943 ksi

Charpy Impact Unnotched 4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F

 

Thermal Properties Metric English Comments
Melting Point 160 °C

320 °F

 

Processing Properties Metric English Comments
Melt Temperature 230 – 260 °C

446 – 500 °F

Mold Temperature 50.0 – 70.0 °C

122 – 158 °F

Drying Temperature 80.0 °C

176 °F

Dry Time 4 hour

4 hour

Moisture Content 0.20 %

0.20 %

Injection Pressure 70.0 – 120 MPa

10200 – 17400 psi