Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties

Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union

Description

Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to the modification. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.15 g/cc

0.0415 lb/in³

Linear Mold Shrinkage 0.0078 cm/cm

0.0078 in/in

Linear Mold Shrinkage, Transverse 0.0093 cm/cm

0.0093 in/in

Melt Flow 2.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
2.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F

 

Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa

16700 psi

Elongation at Break 3.0 %

3.0 %

Tensile Modulus 9.50 GPa

1380 ksi

Flexural Strength 145 MPa

21000 psi

Flexural Modulus 7.85 GPa

1140 ksi

Charpy Impact Unnotched 4.70 J/cm²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F

 

Thermal Properties Metric English Comments
Melting Point 160 °C

320 °F

Deflection Temperature at 1.8 MPa (264 psi) 145 °C

293 °F

Vicat Softening Point 165 °C

329 °F

B
Flammability, UL94 HB

HB

Glow Wire Test 650 °C

1200 °F

 

Processing Properties Metric English Comments
Melt Temperature 200 – 250 °C

392 – 482 °F

Mold Temperature 40.0 – 80.0 °C

104 – 176 °F

Drying Temperature 80.0 °C

176 °F

Dry Time 4 hour

4 hour

Injection Pressure 70.0 – 120 MPa

10200 – 17400 psi